| Corrosion Test Results: Ultra 316L Stainless Steel |
| Test Type |
Alloy |
Test Duration (Hrs.) |
Time For First Rust (Hrs.) |
Percent Rusted Area Test Completion (%) |
| Average |
Range |
| Total Immersion |
316L |
505 |
19 |
5-25 |
18 |
| Total Immersion |
Ultra 316L |
505 |
48 |
25-75 |
6 |
Green Properties
Green strength and density were determined using specimens lubricated with 1% Acrawax C.
Sintered Mechanical and Physical Properties
Sintered mechanical and physical properties were determined on specimens processed in the same manner as Ultra 303L and Ultra 304.
|