Corrosion Test Results: Ultra 304L Stainless Steel
Test Type Alloy Test Duration (Hrs.) Time For First Rust (Hrs.) Percent Rusted Area Test Completion (%)
Average Range
Total Immersion 304L 504 1 -- 22
Total Immersion Ultra 304L 504 480 351-504 1

Green Properties
Green strength and density were determined using specimens lubricated with 1% Acrawax C.



 

 

 





Sintered Mechanical and Physical Properties

Sintered properties were determined using test specimens blended with 1% Acrawax C and compacted to pre-selected pressures. The specimens were delubricated in air for 20 minutes at 950°F, then sintered in dissociated ammonia for 30 minutes at 2100°F and cooled in the water-jacketed furnace cooling zone.